Cold-rolled flat product for panels and skins
Stainless Steel Coil & Sheet
Cold-rolled coil, strip and sheet are commonly used for tank skins, panels, formers and fabricated components. Review width, thickness, finish, slit or sheet format, packaging and handling requirements before quotation.

Standards
- ASTMA240 / A480 (ASME SA-240)
- JISG4305 (cold-rolled)
- EN10088-2 (on request)
Dimensions
- Thickness
- 0.3 - 6.0 mm
- Width
- up to 1500 mm, slit to size
- Form
- Coil · Strip · Sheet
Finishes and applications
- Tank & vessel skins
- Panels, formers & fabricated parts
- Decorative & clad surfaces
Grades and properties
These values are references for quotation review. Actual heat values should be checked against the applicable mill test certificate.
304 / SUS304
ASTM 304 (S30400) / JIS SUS304 / EN 1.4301
Composition, wt %
Minimum mechanical properties
- Tensile strength
- ≥ 515 MPa (75 ksi)
- Yield strength (0.2%)
- ≥ 205 MPa (30 ksi)
- Elongation
- ≥ 40%
- Hardness
- ≤ 201 HB / 92 HRB
Annealed minimums based on ASTM A240 plate and sheet requirements. Tube standards such as A554 may differ; confirm the governing product standard and applicable mill test certificate.
304L / SUS304L
ASTM 304L (S30403) / JIS SUS304L / EN 1.4307
Composition, wt %
Minimum mechanical properties
- Tensile strength
- ≥ 485 MPa (70 ksi)
- Yield strength (0.2%)
- ≥ 170 MPa (25 ksi)
- Elongation
- ≥ 40%
- Hardness
- ≤ 201 HB / 92 HRB
Annealed minimums based on ASTM A240 plate and sheet requirements. Tube standards such as A554 may differ; confirm the governing product standard and applicable mill test certificate.
316 / SUS316
ASTM 316 (S31600) / JIS SUS316 / EN 1.4401
Composition, wt %
Minimum mechanical properties
- Tensile strength
- ≥ 515 MPa (75 ksi)
- Yield strength (0.2%)
- ≥ 205 MPa (30 ksi)
- Elongation
- ≥ 40%
- Hardness
- ≤ 217 HB / 95 HRB
Annealed minimums based on ASTM A240 plate and sheet requirements. Tube standards such as A554 may differ; confirm the governing product standard and applicable mill test certificate.
316L / SUS316L
ASTM 316L (S31603) / JIS SUS316L / EN 1.4404
Composition, wt %
Minimum mechanical properties
- Tensile strength
- ≥ 485 MPa (70 ksi)
- Yield strength (0.2%)
- ≥ 170 MPa (25 ksi)
- Elongation
- ≥ 40%
- Hardness
- ≤ 217 HB / 95 HRB
Annealed minimums based on ASTM A240 plate and sheet requirements. Tube standards such as A554 may differ; confirm the governing product standard and applicable mill test certificate.
430 / SUS430
ASTM 430 (S43000) / JIS SUS430 / EN 1.4016
Composition, wt %
Minimum mechanical properties
- Tensile strength
- ≥ 450 MPa (65 ksi)
- Yield strength (0.2%)
- ≥ 205 MPa (30 ksi)
- Elongation
- ≥ 22%
- Hardness
- ≤ 183 HB / 89 HRB
Annealed minimums based on ASTM A240 plate and sheet requirements. Tube standards such as A554 may differ; confirm the governing product standard and applicable mill test certificate.
Project intake
Need help planning shipment and documentation for Stainless Steel Coil & Sheet?
We provide industrial procurement support through supplier coordination, technical document review and cross-border delivery coordination.